The ElasTek Resiliometer, quickly and accurately measures the “Rubber Property—Resilience by Vertical Rebound” as described in ASTM D2632.
The determination of rebound resilience is accomplished by dropping a plunger of a specific mass and geometry from a predetermined height to the surface of a test specimen and measuring the distance that the plunger rebounds after contact and calculating the ratio of rebound distance to the distance traveled by the mass prior to contacting the test specimen.
This ratio is expressed as a percentage, and since the scale is graduated into 100 equal divisions, this ratio (percentage) may be read directly from the scale when the plunger rebounds to its maximum height.
This instrument is especially useful in developing compounds that are intended to effect the transmission of shock or vibration, as “… resilience is a function of both the dynamic modulus and the internal friction of a rubber.” (ASTM D2632 Section 4).
Ask for Price
- Integral leveling feet and “bulls eye” bubble—in—liquid glass level;
- Height adjustable Pass/Fail Gauge;
- Easy—to—read graduated scale, easily adjusts to specimen height;
- Portable, no power required;
- Quality, billet aluminum base, stainless steel post and other durable components;
- Includes ISO-17025 Certification
Model: | SRI |
Scale: | 0—100 |
Resolution: | 1 point increments |
Total Height: | 559 mm (22 inches) |
Scale Height: | 406 mm (16 inches) |
Width: | 248 mm (9.76 inches) |
Depth: | 241 mm (9.49 inches) |
Specimen Table: | 180 x 115 mm (7.1 x 4.53 inches) |
Jaw Capacity Height: | 89 mm (3.5 inches) |
Jaw Capacity Depth: | 44 mm (1.73 inches) |
Weight: | 7.7 kg (17 lb.) |
Standards: | ASTM D2632 |
Certificate of calibration is included.